Careful control of preheat and interpass temperatures (300o F minimum) are essential to avoid cracking. This filler metal is classified after postweld heat treatment so special care must be taken when using them in the as-welded condition due to higher strength levels.
| Additional Information |
|---|
| Packaging Description:10lb tube |
| Weld Process:TIG |
| Grade:ER80S-B2 |
| Diameter:2.5mm |
| Packaging:10lb tube |
| Brand:Exocor |
| AWS Spec :ER80S-B2 |
| Polarity:DC+ |